<delect id="c0psw"></delect>
    <dl id="c0psw"></dl>
    <center id="c0psw"></center>
    1. <dl id="c0psw"></dl>
    2. 蜜臂在线日本,中文字幕日韩精品一区美,亚洲欧洲精品一区二区,日本特a级毛大片一区二区在线观看

      Welcome to the official website of Shenyang Ruite Titanium & Nickel Technology Co.,Ltd.
      Tubes · Bars · Sheets · WiresAdhering to the spirit of craftsmanship, keep improving.
      Hotline
      +86 13709850972
      Hot Keywords: Titanium bar, Titanium wire, Titanium tube, Titanium plate, Nickel bar, Nickel tube, Nickel wire, Nickel plate, High temperature alloy bar, Forgings
      Location: HOME >>NEWS >>Industry

      推薦資訊

      Contact +86 13709850972

      Manufacturers introduce the factors affecting the use time of titanium alloy rods

      Author: Click:2092 Time:2022-06-10

      The fatigue and fracture properties of titanium alloy rods occupy a very important position in determining the service life of the alloy. Research has been carried out at home and abroad over the years to investigate the fatigue and fracture mechanisms of

      The fatigue and fracture properties of titanium alloy rods occupy a very important position in determining the service life of the alloy. Research has been carried out at home and abroad over the years to investigate the fatigue and fracture mechanisms of titanium alloy rods and their relationship with various metallurgical factors. Due to the complexity of the problem itself and the scattered nature of the initial test data, some of the substantive issues are still not entirely clear and views are not fully unified, so only some representative conclusions are presented here.

      The fatigue life of titanium alloy rods, like that of other materials, depends on the chance of fatigue crack nucleation and the rate of crack expansion. According to the study of pure titanium, fatigue cracks are mostly nucleated in the slip zone and at the twin interface, but for Ti-6AI-4V this type of alloy, under low stress conditions, the a-phase and b-phase interface is the weak link of Z. Only at high stress levels, the chance of nucleation in the slip zone increases significantly, and increasing the test temperature has a similar effect In order to improve the fatigue performance of a ten-b titanium alloy rods, it is usually desirable to obtain a fine equiaxial a ten-b organization, and the b-phase is well free, in order to reduce the a/b-phase interface area. In addition, the fine grain slip is more uniform, slip free distance is short, can reduce the stress concentration caused by dislocation plugging; at the same time, the fine crystal on the twin crystal also has a greater restraint effect. On the contrary, the fatigue strength of coarse crystalline Weiss organization is lower due to the easy nucleation of fatigue cracks. The effect of grain size on the fatigue performance of smooth and notched specimens of Ti-6A1-4V alloy.

      In the presence of notches and stress concentrations, the effect of grain size decreases, as the fatigue life depends mainly on the crack expansion rate, while experimental results for pure titanium show that the crack expansion rate is not closely related to the grain size.

      【相關推薦】

      Return to listRelated labels:
      蜜臂在线日本,中文字幕日韩精品一区美,亚洲欧洲精品一区二区,日本特a级毛大片一区二区在线观看
      <delect id="c0psw"></delect>
      <dl id="c0psw"></dl>
      <center id="c0psw"></center>
      1. <dl id="c0psw"></dl>
      2. 丰宁| 昭觉县| 台东县| 沽源县| 沛县| 宿州市| 日照市| 湘潭县| 邯郸县| 长丰县| 鄄城县| 公主岭市| 清远市| 同心县| 靖远县| 大城县| 井陉县| 龙泉市| 弋阳县| 临夏县| 花莲市| 牟定县| 长武县| 海门市| 垦利县| 江永县| 遂昌县| 德昌县| 墨竹工卡县| 九龙城区| 余庆县| 佛山市| 陆川县| 新龙县| 远安县| 新河县| 太仓市| 镇巴县| 新宁县| 交城县| 桐庐县|